Natural Rubber “Dust Cloth” Strip

Natural Rubber “Dust Cloth” Strip

Metroseal

Price not listed

PROPERTIES TEST METHOD VALUES FPS UNITS TEST METHOD VALUES METRIC UNITS SPECIFIC GRAVITY DIN 53508 1.10±0.05 ASTM D297 1.10±0.05 HARDNESS DIN 53505 40 ± 5 SH A ASTM D2240 40 ± 5 SH A TENSILE STRENGTH ( MIN ) DIN 53504 2350 PSI ASTM D412 165 KG/CM2 ELONGATION AT BREAK ( MIN ) DIN 53504 600% ASTM D412 600% ABRASION RESISTANCE ( MAX ) DIN 53516 120 MM3 ASTM D5963 120 MM3 COMPRESSION SET (70ºC/24 HRS/25% COMPRESSION) (MAX) DIN 53517 30% ASTM D395 METHOD B 30% TEAR RESISTANCE ( ANGULAR ) MIN DIN 53515 224 LBS/INCH ASTM D624 40 KG/CM CHANGE IN PROPERTIES AFTER HEAT AGEING FOR (72 HRS. AT 70 ºC ) AST

Metroseal's own words, read from their page.