Heart & Industry

Home · Metroseal

High Grade Non-reinforced Diaphragm Neoprene Strip

High Grade Non-reinforced Diaphragm Neoprene Strip

Metroseal

Price not listed

PROPERTIES TEST METHOD VALUES FPS UNITS TEST METHOD VALUES METRIC UNITS SPECIFIC GRAVITY DIN 53508 1.40±0.05 ASTM D297 1.40±0.05 HARDNESS DIN 53505 65 ± 5 SH A ASTM D2240 65 ± 5 SH A TENSILE STRENGTH (MIN) DIN 53504 1422 PSI ASTM D412 100 KG/CM2 ELONGATION AT BREAK (MIN) DIN 53504 400 % ASTM D412 400 % COMPRESSION SET (70ºC/24 HRS/25% COMPRESSION) (MAX) DIN ISO 815-1 40% ASTM D395 METHOD B 40% TEAR RESISTANCE (ANGULAR) MIN DIN 53515 95 LBS/INCH ASTM D624 25 KG/CM CHANGE IN PROPERTIES AFTER HEAT AGEING FOR (72 HRS. AT 70ºC ) ASTM D573 HARDNESS (PTS) + 5 (MAX) + 5 (MAX) TENSILE STRENGTH (%) + 10

Metroseal's own words, read from their page.

Buy from METROSEAL LTDPrice seen 2026-09-26. Not an affiliate link, we earn nothing from it.